GRADE : S32205
SURFACE : BLACK/BRIGHT
LENGTH : 6000/5000--7000mm
SHAPE : round/squre/hexagon/bar/rod
Description : stainless steel bar
Material : duplex stainless steel
Stainless steel bar
Equivalent designations
UNS S32205
DIN W. Nr. 1.4462
| Form | ASTM | |||||||||
| Rod, bar and shape | A 276, A 484 | |||||||||
| Plate, sheet and strip | A 240, A 480 | |||||||||
| Seamless and welded pipe | A 790, A 999 | |||||||||
| Seamless and welded tubing | A 789, A 1016 | |||||||||
| Fitting | A 815, A 960 | |||||||||
| Forged or rolled pipe flange and forged fitting | A 182, A 961 | |||||||||
| Billet and bar for forging | A 314, A 484 | |||||||||
| Chemical composition | ||||||||||
| % | Fe | Cr | Ni | Mo | C | Mn | Si | P | S | N |
| min | balance | 22 | 4.5 | 3 | 0.14 | |||||
| max | 23 | 6.5 | 3.5 | 0.03 | 2 | 1 | 0.03 | 0.02 | 0.2 | |
| Physical properties | ||||||||||
| Density | 7.69 g/cm3 | |||||||||
| Melting range | 1385-1443℃ | |||||||||
Features:
2205 is a duplex stainless steel with nearly equal proportions of austenite and ferrite when properly heat treated. This microstructure makes it much more resistant to stress corrosion cracking than stainless steel 304 and 316L. 2205’s higher chromium, molybdenum and nitrogen contents give it significantly improved pitting and crevice corrosion resistance in the presence of chlorides. Its yield strength is about twice that of austenitic stainless steels. It is highly suitable for Applications in environments containing chlorides and hydrogen sulfide such as marine applications and oil and gas production.
Applications:
Oil and gas industry piping, tubing and heat exchangers; pulp and paper industry bleaching equipment, liquor tanks and digesters; cargo tanks for ships and trucks; chemical processing industry pressure vessels, tanks, piping and heat exchangers; and food processing equipment.
|
|
2205 S32205 Stainless Steel Bar Round / Square / Hexagon Shape Stress Corrosion Resistant Images |